A:The following situation will affect the final quality of the film during lamination.
1. Using metal ink
2. Ink containing too much wax, dried oil,adhesive, silicon additive and so on.
3. Much too thick ink
4. Ink completely not dried yet.
5. Much too humid paper sheet.
6. Too much powder on the surface